1737F Corning optical glass properties

Properties of 1737F Glass

Principal use of Corning 1737F optical glass are:


Substrates for flat:

  • Panel displays
  • Fiber and mirror coatings
  • Microelectronic applications
  • Optical windows
  • Electroluminescent displays
  • Optoecetronics

Thermal/Mechanical Properties:

  • Density (at 25 °C/77 °F): 2.54 g/cm3
  • Thermal Coefficient of Expansion (0/300 °C; 32/572 °F): 37.6 x 10 -7/°C; 21 x 10-7/°F
  • Strain Point: 666°C/1231°F
  • Annealing Point:721°C/1330°F
  • Softening Point:975°C/1787°F

Optical Properties:

Electrical Properties

  • Dielectric Constant: E= 5.7

 

 

 

 

 